How to verify? Fold one to check the angle (whether the 90-degree fold is crisp) and whether the crease ‘bursts’ (at the fold line); carry out a test fold before mass production (approval required for the first piece). For small-batch verification of creases, produce a sample box before placing an order.
The creases on packaging boxes are a manual process where ‘press one fen too deep and it bursts; press one fen too shallow and it goes awry’: only when the position, depth and temperature are all correct, the box will fold crisply — ask the manufacturer to demonstrate a test fold for you before placing an order.
How should the depth be adjusted? The depth of the crease line (creasing knife, die): if too shallow, the box won’t fold; if too deep, the line will split (crease failure); for thick paper (greyboard, corrugated board), increase the depth; for laminated paper (depending on film thickness), allow for extra margin.
How can crease bursting be prevented? Crease bursting (cracking at the fold line): commonly seen with thick paper and in low-temperature environments (folding boxes in winter); preheating (workshop temperature), deepening the crease line, and selecting the right paper can help alleviate this.
How is the position determined? The position of the crease line: the boundaries of the box walls (width of each side) and the starting point of the flap (the folded edge of the lid); positional misalignment (due to die-cutting errors) will cause the box to be crooked or misaligned.
Whether a box folds neatly or not depends on the crease lines: if the position is off by just one millimetre or the depth is even slightly incorrect, the box will either be crooked or the crease will split — the crease is the box’s ‘joint’. This article clearly explains the key points regarding crease lines.
What is a crease line? A crease line: a groove pressed into the cardboard or greyboard to allow the box to fold along it; the position of the crease line corresponds to the fold edges of the box (each edge has a line).