Ink Coverage: TAC Limits and Set-Off Risk

What is total area coverage? The sum of the ink percentages laid down at a given point, usually expressed as cyan plus magenta plus yellow plus black. A rich black built from 60/40/40/100 sits at 240 percent, and a four-colour photographic shadow can reach 320 or more. The number matters because ink is a film with a thickness, and past a certain point the film stops drying properly and starts behaving like a wet layer on a stack of sheets.

What limits apply on coated board? Sheetfed offset on coated board commonly runs with a TAC ceiling around 300 to 330 percent, and some presses and dryers work comfortably below that. Flexo on corrugated is a different world, where heavy coverage is limited by the anilox and the absorbency of the liner rather than by a TAC number. Digital toner has its own ceiling, lower and more sensitive to large solid areas. The limit is a property of the process, the ink and the drying setup together, not a universal figure.

What goes wrong when coverage is too heavy? Set-off, where wet ink from a printed sheet transfers to the back of the sheet stacked on top of it, marks the reverse face and sometimes the inside of the carton. Blocking, where sheets stick together in the pile. Slow curing, which shows up later as scuffing in the gluing machine or in transit. Mottling in the solids, because a film that thick cannot level. The catalogue of common print defects traces these back to their causes.

How is coverage reduced without changing the look? Under-colour removal and grey component replacement take some of the chromatic ink out of shadows and put the density into black, which lowers the total film while the eye reads the same depth. Design-side moves help as well: replacing a full-bleed dark background with a lighter tint, or moving heavy coverage away from folded edges where the film has to stretch. The visual result is often indistinguishable, and the press behaves differently.

Does heavy coverage cost more? It can, in three places. More ink per sheet is a direct material cost. Slower running to allow drying is a throughput cost. And a higher reject rate from set-off and scuffing is a yield cost. The article on spot versus process colour covers the other side of the same equation, where adding a spot colour may be cheaper than building a colour from four.

How is ink film measured on press? By densitometry on the sheet, and by checking the plate or the file for the TAC value before the plate is made. A prepress check of the PDF takes minutes and catches the problem while it is still a file. Once plates exist, the options narrow to changing the artwork and remaking plates, or accepting slower running and a higher reject rate. The ink systems and their drying behaviour are compared in the guide to water-based, UV, soy and spot inks.

What should a buyer watch for in artwork? A designer working on screen sees colour, not film weight, so backgrounds at 100 percent across four colours look normal in the file. Ask for the TAC value of the darkest area if the design uses dark full-bleed panels, and ask early. Where artwork is fixed and coverage is unavoidably heavy, the practical answers are a matte varnish over the top to protect the surface and a slower press schedule, both of which belong in the quote rather than in a complaint after delivery.

Chengtop prints folding cartons, corrugated boxes and rigid boxes in Wuhan, and we check TAC at prepress before plates are ordered. Send the artwork and the substrate you plan to use and we will flag anything that needs adjusting. Message us with the files.